| Sign In | Join Free | My polstate.com |
|
Brand Name : JINHAIHU
Model Number : DSC-1150B
Certification : ISO
Place of Origin : BEIJING, CHINA
MOQ : 1 set
Payment Terms : T/T, L/C, Western Union, MoneyGram, D/A, D/P
Supply Ability : 20 sets per month
Delivery Time : 5~10 work days
Packaging Details : Carton
Product name : Calorimeter DSC Plastic Differential Scanning Calorimetry Price
Model : DSC-1150B
DSC range : 0~±500 mw
Temperature range : RT ~1150℃
Aluminum crucibles : Φ6.6*3mm (Diameter * High)
Ceramic crucibles : Φ6.6*3mm (Diameter*High)
Customized support : OEM, ODM
Melting and crystallization temperature and enthalpy measuring instrument
Application:
The instrument features:


| Temperature range | RT-1150℃ |
| Temperature resolution | 0.01℃ |
| Heating rate | 0.1~80℃/min |
| Constant temperature | RT-1150℃ |
| Duration of constant temperature | The constant temperature time is unlimited at low temperature; When more than 1000 ℃, it is recommended that a single constant temperature time is less than 30 min |
| Temperature control mode | Heating, cooling, constant temperature, any combination of three modes cycle use, temperature uninterrupted |
| DSC range | 0~±500mW |
| DSC resolution | 0.01mW |
| DSC sensitivity | 0.01mW |
| Working power | AC 220V 50Hz 300W or other |
| Atmosphere control gas | Two-channel gas control by automatic controlled (e.g. nitrogen and oxygen) |
| Gas flow | 0-200mL/min |
| Gas pressure | 0.2MPa |
| Gas flow accuracy | 0.2mL/min |
| Crucible | Aluminium crucible Φ6.6*3mm (Diameter * High),ceramic crucible Φ6.6*3mm (Diameter * High) |
| Calibration standard | With standard material (Indium, tin, zinc, silver), users can adjust the temperature coefficient and enthalpy value coefficient by themselves |
| Data interface | Standard USB interface |
| Display mode | 7-inch touch screen |
| Output mode | computer and printer |
| Design features | Fully closed support structure design, prevent items falling into the furnace body, pollution of the furnace body, reduce the maintenance rate |
|
|
500mw Calorimeter Plastic Dsc Differential Scanning Calorimetry Images |